Quote:
Originally Posted by ol'George
If it was welded and reground back to specks, my concern would be the heat treatment to restore it to the correct hardness. 
|
I emailed Jeff to ask him. He said "I used ER70S TIG filler rod to build the surface up before machining it to the correct size. The repair should be good as new."