today I started the bodywork on the tins. the waves from the stamping press are terrible. with a hammer and dolly and got a few dings and waves out. then the filler will do the rest.



36 grit on the DA. then 80 grit on the file board. there is a few high spots still in them but I'll 2k prime and block them with 180 grit to see how high they are. (hard to tell with the 80 grit marks in them)



2 coats of 2k over the filler . the 2nd coat I thinned to fill the sand marks once it flows out. (flash time was 15min between coats )